Table of Contents
ToggleBitumen 200/300: The Versatile Paving Solution
Introduction to Bitumen 200/300
Bitumen 200/300 is a crucial paving material with a penetration value between 200 and 300, making it highly versatile for various construction applications.
Properties of Bitumen 200/300
It boasts excellent adhesive properties, weather resistance, and durability. Its medium penetration value ensures optimal binding with aggregates, creating strong and long-lasting road surfaces.
Applications of Asphalt 200/300
This grade of bitumen finds extensive use in road construction, particularly for highways, urban roads, and airport runways. It is also utilized in waterproofing applications and as a binder in asphalt mixtures for superior pavement performance.
Benefits of Asphalt 200/300
Durability: It enhances the lifespan of roads by providing a strong and resilient surface that withstands heavy traffic and environmental factors.
Weather Resistance: Its ability to resist moisture, UV rays, and temperature fluctuations ensures consistent performance in diverse climatic conditions.
Cost-Effectiveness: Using Asphalt 200/300 reduces maintenance costs due to its durability and long service life, making it a cost-effective choice for infrastructure projects.
Quality Assurance and Standards Compliance
Manufacturers adhere to strict quality control measures to ensure Asphalt 200/300 meets industry standards and specifications. This includes testing for penetration, softening point, viscosity, and other key parameters to guarantee performance and reliability.
Specification of Bitumen 200/300
BITUMEN 200/300 |
TEST METHOD |
UNIT |
SPECIFICATION |
|
Specific gravity @ 25/25 °c |
ASTM D70 |
Kg/cm³ |
990-1040 |
|
Penetration @ 25°c |
ASTM D5 |
mm/10 |
200-300 |
|
Softening point °c |
ASTM D36 |
°C |
32 |
|
Ductility @ 25°c |
ASTM D113 |
cm |
100 min |
|
Loss on heating(wt) % |
ASTM D6 |
wt % |
1 max |
|
Drop in Penetration after heating % |
ASTM D5-D6 |
% |
37 max |
|
Flashpoint °c |
ASTM D92 |
°C |
177 min |
|
Solubility is CS2(wt) % |
ASTM D4 |
wt % |
99 max |
|
Spot test |
A.a.s.h.o.t102 |
– |
Negative |
Download the Specification of Bitumen 200/300
Download the MSDS of Bitumen 200/300